商品描述
HIPS 韓國錦湖HI-450 耐沖擊級
特性 | 高抗沖 |
應(yīng)用領(lǐng)域 | 其他板材;食品容器;玩具;家用貨品 |
產(chǎn)品參數(shù)
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 熔體流動速率 | 200℃/5kg | ASTM D-1238 | 4.0 | g/10min |
模具收縮率 | Flow | ASTM D-955 | 0.30-0.60 | % | |
吸水率 | 24hr | ASTM D-570 | 0.050 | % | |
物理性能 | 比重 | ASTM D-792 | 1.04 | g/cm3 | |
機械性能 | 拉伸屈服強度 | ASTM D-638 | 40.1 | MPa | |
拉伸屈服伸長率 | ASTM D-638 | 45 | % | ||
彎曲模量 | ASTM D-790 | 2250 | MPa | ||
彎曲屈服強度 | ASTM D-790 | 43.1 | MPa | ||
IZOD缺口沖擊強度 | 3.18mm | ASTM D-256 | 89.1 | J/m | |
洛氏硬度 | ASTM D-785 | 80 | L scale | ||
電氣性能 | 體積電阻率 | ASTM D-257 | 1.0E+16 | ohm.cm | |
介電強度 | ASTM D-149 | 17.7 | KV/mm | ||
介電常數(shù) | 1E+6Hz | ASTM D-150 | 2.700 | ||
熱性能 | 熱變形溫度 | 1.80MPa,未退火 | ASTM D-648 | 82.2 | ℃ |
維卡軟化溫度 | ASTM D-1525 | 101 | ℃ | ||
燃燒性 | 1.59mm | UL 94 | HB | ||
燃燒性 | 3.18mm | UL 94 | HB | ||
燃燒性 | 6.35mm | UL 94 | HB | ||
RTI Str | 1.59mm | UL 746 | 50.0 | ℃ | |
RTI Str | 3.18mm | UL 746 | 50.0 | ℃ | |
RTI Str | 6.35mm | UL 746 | 50.0 | ℃ | |
RTI Imp | 1.59mm | UL 746 | 50.0 | ℃ | |
RTI Imp | 3.18mm | UL 746 | 50.0 | ℃ | |
RTI Imp | 6.35mm | UL 746 | 50.0 | ℃ | |
RTI Elec | 1.59mm | UL 746 | 50.0 | ℃ | |
RTI Elec | 3.18mm | UL 746 | 50.0 | ℃ | |
RTI Elec | 6.35mm | UL 746 | 50.0 | ℃ |